X
Product Description
Feldspar
Test Report
Test Report
- Test Report No.: BALL / 3498/2008
- Issue Data: 28.02.2008
- Your Ref: Nil
- Date: Nil
- Sample Particulars: Feldspar Sample
- Qty: 200g.
- Test Required: As given below
- Date of Registration: 20.02.2008
- Date of commencement of testing: 21.02.2008
- Date of completion of testing: 27.02.2008
- Sample condition at receipt: Found OK
- Sample tested as received
- Sample Method: Sample collected and submitted by the customer
Tests | Results |
Loss on ignition, % by mass | 0.24 |
Silica as SiO2, % by mass | 64.30 |
Iron as Fe2O3, % by mass | 0.15 |
Alumina as Al2O3, % by mass | 19.48 |
Calcium as CaO, % by mass | 0.35 |
Magnesium as MgO, % by mass | 0.20 |
Sodium as Na2O, % by mass | 3.35 |
Potassium as K2O, % by mass | 11.41 |
Titanium as TiO2, by mass | 0.10 |
- Interpretation of Result: Nil
- Deviation from test method and condition: Nil